Test

Preparazione della struttura

  • Prepare the framework in accordance with the criteria specified by the alloy manufacturer.
  • Depending on the manufacturer pecifications, oxidation firing must be carried out..
  • Once oxidation firing has been completed, the metal surface must be sandblasted with 110μm and approx. 2-3 bar pressure.
  • Afterwards, the metal surface may no longer be touched.
  • Clean with pressurized air.

Survey of alloys tested and approved with VITA NP BOND Paste

* Positive results are now also available with WIROBOND® 280 (BEGO), ceramill sintron® (AmmanGirrbach), KERA®-DISC (Eisenbacher Dentalwaren) and Solera Cam® (Dentale Kompetenz®). Please use the VITA alloy list to verify whether your alloy has also been successfully tested with a VITA ceramic.